| WSF / Nylon12 - Dying Tip [message #49909] Sat, 16 June 2012 09:16 UTC |
 |
|
Hi everyone
Recently I met with a range of different technicians from a variety of establishments.
One tip from a German company was that during the dying process they put it in a vac chamber, this draws the dye deeper into the part.
Since i don't have a vac chamber to hand i cant test this.
But if any ones does, could they please post.
boop
|
|
|
|
| Re: WSF / Nylon12 - Dying Tip [message #49912 is a reply to message #49909 ] Sat, 16 June 2012 12:23 UTC |
 |
|
Really not sure.
Regrettably id had a few drinks by that point and didnt question him further on the process.
I'm going to suggest it when I visit another university next week.
See if i can give them a model and some dye, then let them have a test.
I presume they would have a way of agitating the dye while in the vac-chamber or perform a series of vacuuming and agitating separately.
boop
|
|
|